Note1: if the ductility at 25°C (77°F) is less than 100, The material is still acceptable if its ductility at 15°(59°F) is more than 100
Designation MC-30 MC-70 MC-250 MC-800 MC-3000
Min Max Min Max Min Max Min Max Min Max
Kinematic viscosity at 60°C (140°F),mm2/s 30 60 70 140 250 500 800 1600 3000 6000
Flash point (Tag open cup), °C(°F) 38(100) ... 38(100) ... 66(150) ... 66(150) ... 66(150) ...
Distillate Test: Distillate, Volume Percent of Total Distillate to 360°C (680°F):
to 225°C(437°F) ... 35 ... 25 ... 20 ... ... ... ...
to 260°C(500°F) 30 75 10 70 5 55 ... 40 ... 15
to 316°C(600°F) 75 95 65 93 60 90 45 85 15 75
Residue from distillation to 360°C (680°F) 50 ... 55 ... 67 ... 75 ... 80 ...
Percent Volume by Difference Tests on Residue from Distillation:
Viscisity at 60°C (140°F),P 30 120 30 120 30 120 30 120 30 120
Ductility at 25°C(77°F), cm 100 ... 100 ... 100 ... 100 ... 100 ...
Solubility in trichlomethy lene, % 99.0 ... 99.0 ... 99.0 ... 99.0 ... 99.0 ...
water, % ... 0.2 ... 0.2 ... 0.2 ... 0.2 ... 0.2
Instead of viscosity of the residue , the specifying agancy, at its option , can specify penetration 100g: 5 s at 25 C(77°F) of 120 to 300 for MC-30, MC-7, MC-250 grades and 120 to 250 for MC-800 and MC-3000 However, in no case, will both be required. Editorially corrected to match originally published D2027-97.